A-286 (UNS S66286/W. Nr.1.4980) is an iron-nickel-chromium alloy with
additions of molybdenum and titanium. It is agehardenable
for high mechanical properties. The alloy
maintains good strength and oxidation resistance at
temperatures up to about 1300°F (700°C). The limiting
chemical composition is given in Table 1. The alloy is
austenitic in all metallurgical conditions.
The high strength and excellent fabrication
characteristics of INCOLOY alloy A-286 make the
alloy useful for various components of aircraft and
industrial gas turbines. It is also used for fastener
applications in automotive engine and manifold
components subject to high levels of heat and stress and
in the offshore oil and gas industry.